Slant 3D posted a short today showing the cheapest fix for sagging holes: a tiny chamfer on the top edge. Here is why that works, when it does not, and how to tell a sag problem from a size problem.

Slant 3D posted a short today with advice that is older than most slicers and still beats half the settings people fiddle with: give the top of your hole a small corner. A shallow chamfer on the upper edge of a hole, made in the CAD model, lets the hole hold its shape while printing. No extra supports inside the hole, no per-filament tolerance hacking, no reprinting until it happens to fit.

Why the top of the hole is the weak point

A printed hole is not one feature, it is a stack of tiny bridges. Every wall line near the top of the hole crosses open space on its way around, and the final turns have nothing under them but air. Molten plastic sags toward gravity until it cools, so the last few layers droop into the opening. The hole that measured fine in the model comes out undersized, oval, or with a lip you can feel with a fingernail. Mating pins sag too, just in the opposite direction, and a bad fit is usually half hole and half pin.

This is why chasing the problem in tolerance settings is often wasted effort. Compensation cannot un-sag a bridge. If the top of the hole physically collapses inward, every correction value you set gets overwritten by physics on the last few layers.

The design fixes come first

The chamfer works because it turns a sharp, unsupported edge into a gentle slope. Each new contour has a little bit of previous layer to land on instead of nothing at all. Shallow is the instruction, a chamfer you would barely notice in the model is enough, and it stays outside the tolerance zone of the fit itself. While you are in the CAD, add support under the pin that goes into the hole. Slant 3D's note on that is blunt: a supported pin stays crisp, an unsupported one sags and eats your clearance from the other side.

Two more design habits cost nothing. Orient so the critical hole points up, that is the direction the sag problem is worst but also the direction that is cheapest to fix with a chamfer. And if the hole is a press fit, model the real clearance from the start. Prusa's design guidance puts a first usable clearance for moving printed parts at around 0.3 mm, and that number assumes the hole is printing clean, not collapsed.

How to tell a sag problem from a size problem

Print a small test part with upright holes in two or three sizes, in the filament and profile you actually use. Let it cool to room temperature, then measure with inside caliper jaws at three angles and average. Bambu Lab's calibration notes say this honestly: hole calibration is specific to each filament, so test with the one that matters. Measure away from the first layer, or you are measuring elephant foot, not the hole.

Now read the pattern. Same shortfall in millimeters at every hole size is a constant error, and that is what compensation settings are for. Error that grows as the holes get bigger, as a percentage, is thermal shrinkage, and you fix that with shrinkage compensation in percent, not with hole offsets. Only the bottom layers wrong is first layer squish, a Z offset and elephant foot problem. And if the hole measures different across X than across Y, stop calibrating temperature and go check belt tension.

The compensation settings, by slicer

For a confirmed constant error, the math is simple and one thing surprises people: the setting moves each wall, so the diameter changes twice as much as the value. A 5.00 mm hole measuring 4.80 mm needs plus 0.10 mm of hole compensation, added to whatever value is already in the profile.

OrcaSlicer and Bambu Studio put X-Y hole compensation under Process, Quality, Precision. Positive opens holes, and a separate contour setting handles outside walls. Cura has Hole Horizontal Expansion in the Walls category, positive opens holes, and beware the trap: plain Horizontal Expansion works with inverted intuition, there a positive value makes holes smaller. PrusaSlicer has no hole-only setting at all as of 2.9.x, the community has asked for one and Prusa has tracked it as a duplicate request with no commitment. The options are XY Size Compensation, which moves every edge in the model including the outside walls, a negative volume used as a resizable hole, or resizing the hole in CAD.

Know the limits before trusting a value. Hole compensation applies to closed paths only, and on holes with a side opening it creates visible layer separation at the hole, per Bambu's wiki. Sub-millimeter holes tune badly on any machine. And a thread is not a test: an M6 screw made to normal ISO tolerances measures closer to 5.9 mm, so judge fit with gauge pins or a test part, not the hardware bin.

The order that actually works

Chamfer the hole edge and support the pin. Measure the cooled print. Diagnose which error you have. Change exactly one setting. Reprint. Most sagging holes that land on a forum with a screenshot of a failed fit are a missing chamfer, not a missing half-tenth. Fix the geometry, then fine tune the number.