HP's Formnext press release buried its most consequential section. Alongside MJF roadmap news, HP laid out four Metal Jet material collaborations: CM247LC and IN718 nickel superalloys, commercial pure copper, and tungsten carbide production.

HP's Formnext 2026 announcement led with the MJF 1200 availability dates and a 20 percent productivity mode for the Jet Fusion 5600 line. We covered both. But the part of the press release that actually changes what factories can produce has nothing to do with new machines. HP used the show to detail a Metal Jet material expansion spanning nickel-based superalloys, pure copper and tungsten carbide, with a named partner for each. The S100 binder jet printer was not the news. The powders were.

Four collaborations, four different credibility problems

Superalloys first, because they are where binder jetting has the most ground to make up. HP worked with Alloyed, the UK rapid-diffusion-bonding specialist based in Yarnton, on CM247LC, a directionally solidified cast superalloy used in turbine hardware. The partners report densities above 98 percent of theoretical on Metal Jet parts, and they went beyond coupons: Alloyed ran a turbine-wheel benchmark to prove complex geometry holds together at high temperature.

The second superalloy story is different in kind, and arguably more useful. HP qualified IN718 with IndoMIM, a foundry in Karnataka, India, and published an actual technical data sheet. The numbers: approximately 1,369 MPa ultimate tensile strength, 1,145 MPa yield strength, and 20 percent elongation after heat treatment. A demo part proves a machine can do something once. A data sheet with batch-level mechanical properties is what a design engineer can put into a stress calculation, and what a qualification auditor can sign.

Pure copper is the commercial one. HP says pure copper parts are available now from Dauch's facility in Auburn Hills, Michigan, aimed at thermal management and electrification work. Copper has become the hardest material in the building, both because of laser reflections and because demand from AI server cooling and EV motors is outrunning capacity. A production route that skips the laser entirely has a structural advantage here, and Dauch selling printed copper as a service today is the proof.

Tungsten carbide closes the set. HP and Hyperion Materials and Technologies have a Strategic Preferred Partner Agreement from October, and the first production Metal Jet S100 for carbide is already installed in Barcelona. Carbide is where the value math works without apology: tooling and wear parts are small, expensive, and geometry-limited in ways pressing and grinding cannot escape.

The moat is powder specs, not print speed

Worth being blunt about what this announcement is really doing. Binder jetting's powder requirements diverge from laser powder bed fusion: tighter particle size distribution control, a sintering window that survives debinding and furnace steps, batch-to-batch consistency that survives all of it. Every one of these four collaborations is, at bottom, a powder qualification effort. That is also why the timing matters. The stainless grades Metal Jet shipped on were never the barrier to adoption; aerospace and energy buyers stayed out because there was no qualified superalloy path and no data sheet to qualify against.

HP also previewed AI work at the show: in-situ process monitoring from imaging and thermal data to predict defects, a service chatbot, and maintenance prediction from printer telemetry. No dates, no products. Skip it for now and watch the powder supplier qualification lists instead. Whichever grade gets HP certification first locks in supply eligibility for the whole route, and that is where the next two years of this market will be decided.

For anyone who argued in 2026 that binder jetting stayed a niche for steel and steel-adjacent parts, this press release is the counterexample to file. The machine has been capable for a while. HP just spent a year getting the materials paperwork done.

Disclosure: Some links are affiliate links. We may earn a small commission at no extra cost to you.